Home | SLS | Materials | Request a Quotation | Case Studies | Contact



LaserForm ST200 material enables the manufacture of complex fully dense usable metal parts in a matter of days. Final composition is approximately 46% bronze and 54% 420 stainless steel.
General Properties | Value | Test |
Specific Density | 6.73 g/cm3 | ASTM D792 |
Mechanical Properties | Value | Test |
Tensile Yield Strength (0.2%) | 250 MPa | ASTM E8 |
Tensile Strength | 435 Mpa | ASTM E8 |
Tensile Modulus | 137 GPa | ASTM E8 |
Elongation | 6% | ASTM E8 |
Compression –Yield Strength | 277 MPa | ASTM E8 |
Hardness, Rockwell B (as infiltrated) | 79 | ASTM E18 |
Hardness, Rockwell B (as machined) | 73 | ASTM E18 |
Thermal Properties | Value | Test |
Thermal Conductivity @215°C | 39 w/m°C | ASTM E457 |
Coefficient of Thermal Expansion x10-6 (51-150°C) | 7.45 m/m/°C | ASTM E831 |
Data was generated by building parts under typical processing conditions: |
|
|